The quartz recoveries at pH 10.5 with amide-amine were higher than those with etheramine in all the tested concentrations. At pH 10.5, the selective window in flotation of quartz from hematite was of 80%. The presence of secondary amide in the chemical formula of the reagent was identified through amide-amine infrared spectrum …
Pure quartz flotation showed that all ILs had excellent collection performance, exceeding 95% of the quartz was floated below the concentration of 8*10⁻⁵mol*L⁻¹. All ILs showed much better ...
The poor flotation of coarse quartz particles (>0.150 mm) causes significant problems in various iron ore flotation circuits by contaminating the concentrate. The study evaluated the performance ...
The present study investigates the optimization and advanced simulation of the flotation process of coarse particles (–425 + 106) using micro-nanobubbles (MNBs). For this purpose, flotation …
In this study, the effect of ultrasound (US) on the quartz-amine flotation system was investigated in detail by considering various surface chemistry techniques. The effect of ultrasound on particle size, shape factor, and surface roughness were characterized by using Brunauer-Emmett-Teller (BET) surface area measurements and scanning electron ...
Flotation tests were conducted by using kyanite and quartz single minerals. The effect of pH on the flotation recovery when using 3.0 × 10 −4 mol L −1 sodium petroleum sulfonate (SPS) as the collector is shown in Fig. 1.Kyanite recovery increased significantly with pH and reached a maximum of 58% at pH 4 and then started to decrease.
The use of quartz sand. Quartz sand is an important industrial mineral raw material, non-chemical dangerous goods. Industrial production is generally 50KG or 25KG packaging and export ton bag packaging. Common specifications: 0.5-1.0mm 0.6-1.2mm 1-2mm 2-4mm 4-8mm 8-16mm 16-32mm. (mm is millimeter unit) Common application …
The SiO2 H2O interface and effects on quartz activation in flotation system. Zhongxi Sun, W. Forsling, Jingsheng Chen. Published 1992. Materials Science, Chemistry. Transactions of Nonferrous Metals Society of China. The correlation between surface complexation at the SiO sub 2 H sub 2 O interface and quartz flotation behavior was studied.
Flotation is a method that enables the separation of hydrophobic particles with the help of air bubbles (Fig. 3 a). In flotation, the particles adhere to air bubbles depending on solid, liquid, and gas contact phases. The interaction of particles and bubbles includes collision, adhesion, and stability [ 3, 4, 5 ].
The flotation results suggested that NaAl could inhibit the flotation of Ca²⁺-activated quartz in sodium oleate (NaOl) system to different degrees, depending on the addition sequence of NaOl ...
3.2 Flotation Tests 3.2.1 Single Mineral. Figure 1 shows the recovery of each mineral in the sink fraction during flotation at pH 9 with 1.5 kg/t Q-amine. The phosphate showed the highest recovery of 93.4%, and a glauconite recovery of 88.2%, while the quartz recovery was 7.5%. The high recovery of phosphate is due to the presence of …
Abstract: The purity of a quartz ore is relatively low at a SiO2 content of 97.18%, and the main impurity in the ore is Fe, Al, and Ca bearing minerals. The main component in an industrial waste bacteria (WJ) is polysaccharides, which may be used as depressors for inhibiting iron minerals in quartz flotation. Moreover, WJ belongs to …
The micro-flotation tests with mineral mixtures showed that through biotreatment, it became possible to float the hematite and depress the quartz particles [13]. Patra and Natarajan in 2004 ...
During practical production, siderite has an influence on flotation efficiency to hematite and magnetite. In flotation system of dodecylamine, this paper studied the flotation properties of single minerals such as magnetite, martite and quartz firstly. On this basis, the influence of siderite to flotation efficiency of martite-quartz and magnetite …
The results of flotation and adsorption tests showed that the effect of siderite on quartz flotation is related to the dissolved siderite species and starch, and siderite significantly influences ...
In this work flotation and single bubble tests were conducted with high purity quartz in water and hexylamine solutions at different pHs. It was found that flotation kinetics and time of the three-phase contact (TPC) formation (t TPC) at the quartz surface by the colliding bubble were affected by the hexylamine concentration and the solution …
Quartz is often symbiotic with feldspar silicate minerals, which is difficult to separate and purify because of their similar physical and chemical properties. Flotation is the most effective method for the separation of quartz and feldspar. The main flotation methods for the separation of quartz and feldspar, such as hydrofluoric acid method, …
Primary monoamines have been long used and studied as flotation collectors for quartz. In the past several mechanisms have been proposed to explain the manner in which the amines adsorb onto and render the mineral hydrophobic and, thus, floatable. From past data and proposed mechanisms and reinterpreting some of the past …
The flotation separation of muscovite from quartz was investigated using mixed sodium oleate/dodecylamine acetate (NaOL/DDA) collectors. The experiments were conducted on single minerals and on a ...
Hydrogen bonds play an important role in the interaction between surfactants. In this study, the effect of three different ethoxylated alcohols (OP-10, NP-10, AEO-9) on the collecting behavior of sodium oleate (NaOL) in the flotation of quartz was investigated. To explore the mechanism, the hydrogen bond between ethoxylated …
Quartz, the second most abundant mineral in the earth's crust, is a gangue mineral in practically every flotation process. Coarse quartz flotation has been a long standing problem in various ...
The micro-flotation of quartz particles was performed using an XFG-cell in the presence and absence of BMNBs with Cetyltrimethylammonium bromide (CTAB) as a collector. The characterization of bubble sizes showed that the bulk micro-bubble (BMB) and bulk nanobubble (BNB) diameters ranged from 1–10 μm and 50–400 nm, respectively.
Given the strong polarity of the quartz surface, it is easy to hydrate to form a hydroxylation layer, which makes it impossible to float quartz with sodium oleate (OL) used alone. An ideal flotation method …
The results demonstrated that it was more likely for quartz with higher fluid inclusion abundance to connect with Fe3+ sufficiently to achieve a high level of flotation recovery, …
Coarse quartz flotation has been a long standing problem in various mineral processing plants to reduce milling cost and increase valuable mineral recovery. Based on this, the effects of nanobubbles (NBs) and hydrodynamic parameters on coarse quartz particle flotation were systematically investigated. Mechanical flotation experiments …
The flotation results suggested that NaAl could inhibit the flotation of Ca²⁺-activated quartz in sodium oleate (NaOl) system to different degrees, depending on the addition sequence of NaOl ...
The flotation responses of quartz and feldspar with alkylsulfonates' collectors in the presence of some alkaline earth metals were studied. The activation mechanism in these systems is discussed in terms of hemimicellization and surface precipitation of neutral component of cation-sulfonate complex, e.g. Ca(OH)RSO 3.. Selective flotation of …
Selective flotation of quartz from feldspar using hydroxypropyl starch as depressant - ScienceDirect. Download full issue. Minerals Engineering. Volume 195, …
After adding the collector, and adjusting the pulp for 1.5 min, flotation scraping bubble was conducted for 5 min. Referring to the reverse flotation process of Anshan-type hematite, the artificially mixed minerals samples were prepared by mixing the mass ratio of quartz and hematite at 2/3, which the iron grade was about 41.27%.
The flotation recovery of quartz remained constant within the addition range from 0 to 140 mg/L for WS and G50, while for NS the quartz recovery remained the same within the addition range from 0 to 40 mg/L and then gradually decreased to 70.25% at the addition of 140 mg/L. In contrast, the flotation recovery of hematite was dramatically ...